Gold processing

Hey guys this is just part one of two. I had to split it because its going to be like a 35 minute video. Let me know what you think!There is an error in the video where i say 2:1 but 3:1 is written. The correct one is 2:1

Comments

It should be up tomorrow

Nile Red

When do u think you'll post the mercric chloride video

I really forgot to mention this part. The copper/nickel solution from the first part can be recycled and used to "wash" more PCBs. I totally spaced on the disposal/usage of the waste liquid... The aqua regia waste is disposed of. Aqua regia loses it's strength pretty quickly.

Nile Red

What about the other metals on a PCB like copper etc, do they just get thrown out with the Aqua Regia mix?

Next video: 1000kg computer parts

Nile Red

Thanks for this! I actually own an IT company and have been giving all our scrap parts away for free for years (knowing they had Gold in them). Time to scale up your method to some 20l drums I think!!